A few small pieces of my kiln apparently fell onto my glass when I closed the lid prior to fusing. Any way to remove them from the fused glass?
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Pieces of kiln stuck in fused glass

Post by Marty »

Drill, grind, or sandblast them out, fill with frit or something else and refire.
Or cut the offending parts out and reuse the clean pieces.

More important- if they didn't come from dropping the lid (you should have opened and checked before firing), you need to fix whatever's causing the debris.