2 way mirror

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

2 way mirror

Post by Bert Weiss »

does anybody have experience kiln carving with 2 way mirror?
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: 2 way mirror

Post by Buttercup »

Don't you love it when someone who's never done something offers advice :roll: ? I've never done it but my guess is that the silvering would fry/melt off, unless the kiln stays under the temperature that the molten tin would be when the glass is floated on it. Please report back if you try it. Jen
Post Reply