Patty Gray Mold

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Deb
Posts: 7
Joined: Sun Feb 22, 2004 11:12 pm

Patty Gray Mold

Post by Deb »

I just purchased one of the Patty Gray Dam Mold. I kiln washed it and then found some instructions on the web that indicated to use boron nitrate. Is kiln washed and then lining with shelf paper ok to use?
Marty
Posts: 863
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Patty Gray Mold

Post by Marty »

Boron nitrate ain't. You'll want boron nitride but if this is a ceramic mold then I don't know why kiln wash won't work. Lining with shelf paper before firing will most likely get you a lump of crumpled fiberpaper in the bottom of the mold, stuck to the glass in ways you won't like.
However, I haven't gone through the tutorial........
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Patty Gray Mold

Post by JestersBaubles »

Love the PG Dam molds. Use them per the directions and you will have good success. That being said, I think kiln wash would be fine, but do line the bottom with Papyros or Thinfire.

2 cents,

Dana W.
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Patty Gray Mold

Post by jim burchett »

Why not Ask Patty?
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie