Patty Gray Mold
Moderators: Brad Walker, Tony Smith
Patty Gray Mold
I just purchased one of the Patty Gray Dam Mold.   I kiln washed it and then found some instructions on the web that indicated to use boron nitrate.   Is kiln washed and then lining with shelf paper ok to use?
			
			
									
						
										
						Re: Patty Gray Mold
Boron nitrate ain't.  You'll want boron nitride but if this is a ceramic mold then I don't know why kiln wash won't work.  Lining with shelf paper before firing will most likely get you a lump of crumpled fiberpaper in the bottom of the mold, stuck to the glass in ways you won't like.
However, I haven't gone through the tutorial........
			
			
									
						
										
						However, I haven't gone through the tutorial........
- 
				JestersBaubles
 - Posts: 705
 - Joined: Fri Feb 25, 2011 12:01 am
 - Location: North Logan, UT
 - Contact:
 
Re: Patty Gray Mold
Love the PG Dam molds. Use them per the directions and you will have good success. That being said, I think kiln wash would be fine, but do line the bottom with Papyros or Thinfire.
2 cents,
Dana W.
			
			
									
						
										
						2 cents,
Dana W.
- 
				jim burchett
 - Posts: 255
 - Joined: Sun Jun 29, 2003 4:24 pm
 - Location: Lenoir, NC
 
Re: Patty Gray Mold
Why not Ask Patty?
			
			
									
						