Lytherm 1/16" Fiber Paper

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
lbailey
Posts: 86
Joined: Fri Oct 26, 2012 2:53 pm
Location: FL Panhandle

Lytherm 1/16" Fiber Paper

Post by lbailey »

I have been given a 200 'x 2' x 1/16" roll of Lytherm 550-LF fiber paper the original owner apparently bought for use in a glass kiln, but never used. MSDS online has the expected precautions about inhalation and handling hazards for this kind of material. I found a spec sheet here: http://www.fabricationspecialties.com/p ... m550-L.pdf

Seems suitable for insulation up to 2300 F, but really want to know if anyone has used it in kiln forming as a base for the powder crackle technique, or any other purpose? I obviously have a bunch of it and want use it (safely) if possible.

Also, what would be a safe testing approach for this?

Thanks
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Lytherm 1/16" Fiber Paper

Post by Brad Walker »

It's a good quality fiber paper. Use same precautions as any other fiber paper. Should work well for crackle, for lining dams, or similar use.

Wish somebody'd give me a roll.
lbailey
Posts: 86
Joined: Fri Oct 26, 2012 2:53 pm
Location: FL Panhandle

Re: Lytherm 1/16" Fiber Paper

Post by lbailey »

Thanks Brad. Luck counts......
Post Reply