remove fired liquid bright gold

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

remove fired liquid bright gold

Post by rosanna gusler »

hi there . i have a bowl with thompsons liquid bright gold fired on and i want to take it off. i can not remember if sulphuric or nitric is the acid of chouce. help? rosanna
artist, owner of wanchese art studio, marine finisher
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: remove fired liquid bright gold

Post by Kevin Midgley »

BonAmi cleaner will remove it.
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: remove fired liquid bright gold

Post by Brad Walker »

Nitric acid, usually as aqua regia (which is a nitric and hydrochloric mixture), but nitric alone will do it. I don't think sulfuric acid will dissolve gold unless it's really concentrated.

I suspect sandblasting would work, too.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: remove fired liquid bright gold

Post by Bert Weiss »

In the stained glass world, black patina is nitric acid. All I know is that this dissolves vitreous enamels. I would guess it works on gold.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions