Hi all... good to see you all still here!
I wish to mount thick cast glass - like dalles, but glass cast and stained in my kilns, 15-25mm thick - in a resilient framework, able to withstand occasional vibration. The Liverpool Metropolitan Cathedral has its acres of glass set in a sort of black rubbery matrix, which would be perfect! But - what is it? It looks rather like the rubbery stuff that they lay down under the play equipment in children's playgrounds.
			
			
									
						
										
						architectural glass mounting ... rubber/epoxy?
Moderators: Brad Walker, Tony Smith
- 
				tonyroberts
 - Posts: 23
 - Joined: Thu Dec 16, 2004 5:59 pm
 - Location: Liverpool UK
 - Contact:
 
- 
				DonMcClennen
 - Posts: 381
 - Joined: Sun Mar 09, 2003 9:09 pm
 - Location: Ontario
 
Re: architectural glass mounting ... rubber/epoxy?
I'm thinking it might be a form of a material like Thiokol which is black and is/was used to install car windshields... flexible and very strong..
			
			
									
						
							"The Glassman"
			
						- 
				tonyroberts
 - Posts: 23
 - Joined: Thu Dec 16, 2004 5:59 pm
 - Location: Liverpool UK
 - Contact:
 
Re: architectural glass mounting ... rubber/epoxy?
Thanks.... but no, this stuff is two-three inches deep, more like the dimensions of the concrete in modern architectural stained glass panels. 
??? Tony
			
			
									
						
										
						??? Tony
- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: architectural glass mounting ... rubber/epoxy?
You can get silicone epoxy that comes in 2 parts.  Some are clear and others not.  
I am a fan of using L screws. They are minimally visible, and will not let the load fall off.
			
			
									
						
							I am a fan of using L screws. They are minimally visible, and will not let the load fall off.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Valerie Adams
 - Posts: 587
 - Joined: Mon Apr 19, 2004 2:49 pm
 - Location: Santa Rosa, California
 - Contact:
 
Re: architectural glass mounting ... rubber/epoxy?
You can get black flexible grout but that's assuming the glass is mounted to something I believe.