Kiln residue

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Jylaine O'Neal
Posts: 1
Joined: Tue Jul 26, 2005 12:51 pm
Location: Ruidoso, NM

Kiln residue

Post by Jylaine O'Neal »

I've been happy with a kiln my husband made many years ago, but it is now raining residue on my glass. It has fiber blanket on the sides and top. I have to sand blast everything to get a smooth surface now. It has been cleaned with a vacuum. Is there anything that can be done to fix the problem, or is it time for a new kiln? One of my friends has a ceramic brick kiln with the same problem, and has to put a propped up kiln shelf over her piece, to keep it from getting dirty. Seems like there must be a better answer.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Kiln residue

Post by Buttercup »

If it's a home-made kiln you can probably simply change the lid liner to a sheet of Ceramaguard. See Kevin's post two posts down. (for some reason the link won't paste). If you want to see a lid rebuild using Ceramaguard I'll find a post I made a couple of years ago. Hope that helps. Jen