kiln side elements not working

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Deb Brown
Posts: 8
Joined: Tue Nov 19, 2013 10:42 am

kiln side elements not working

Post by Deb Brown »

I have an Evenheat Rampmaster II, GTS 23-13. The side elements are not coming on when I fire. The lid element works fine. I just ordered new elements and replaced them, turned kiln on, and grrr, they are still not coming on. I do not understand what is going on, I am stumped, ----anyone with advise or input??? I need HELP...
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: kiln side elements not working

Post by Tony Smith »

Sounds like a failed relay.

Buy a pair and replace them both.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Arnold Howard
Posts: 47
Joined: Mon Oct 13, 2003 5:21 pm
Location: Converse, Texas USA
Contact:

Re: kiln side elements not working

Post by Arnold Howard »

I agree that the relay has probably failed. A relay is a switch that turns on the elements. The temperature controller turns on the relays. The heating elements in a glass kiln rarely fail. It is almost always a relay. The exception is the elements in crucible kilns.

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com
Deb Brown
Posts: 8
Joined: Tue Nov 19, 2013 10:42 am

Re: kiln side elements not working

Post by Deb Brown »

Thank you for your input Tony and Arnold - I will look into replacing the relay(s), this makes sense to me .
Arnold Howard
Posts: 47
Joined: Mon Oct 13, 2003 5:21 pm
Location: Converse, Texas USA
Contact:

Re: kiln side elements not working

Post by Arnold Howard »

Deb, the problem could also be a disconnected wire. A multimeter would help determine why the elements are not turning on.

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com
Deb Brown
Posts: 8
Joined: Tue Nov 19, 2013 10:42 am

Re: kiln side elements not working

Post by Deb Brown »

thanks, input re thermocouple very useful, really appreciate being able to get advise, :)
Last edited by Deb Brown on Tue Feb 02, 2016 6:56 pm, edited 1 time in total.
Deb Brown
Posts: 8
Joined: Tue Nov 19, 2013 10:42 am

Re: kiln side elements not working

Post by Deb Brown »

Thanks Arnold, I have a multimeter. I will open up the kiln electrical again and take a look at everything, see what I can see, test what I can test. :)
Brad Walker
Site Admin
Posts: 1540
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: kiln side elements not working

Post by Brad Walker »

Deb Brown wrote:Tony and or Arnold - I just looked in my kiln owners manual, kiln maintenance, and it does not show me a relay. I am not sure what a relay would look like, is this different than the thermocouple? Where in the kiln would the relays be? In the electrical connections area where the leads come from the controller , or in the controller itself. What do they look like?
The relay is inside the controller box.

It looks like this: https://shopevenheat.com/index.php?main ... ts_id=1484
Arnold Howard
Posts: 47
Joined: Mon Oct 13, 2003 5:21 pm
Location: Converse, Texas USA
Contact:

Re: kiln side elements not working

Post by Arnold Howard »

Deb, please be very careful with a multimeter. If you test the connections with the kiln plugged in, you will be exposed to live wires.

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com
Deb Brown
Posts: 8
Joined: Tue Nov 19, 2013 10:42 am

Re: kiln side elements not working

Post by Deb Brown »

Hi Arnold, Brad and Tony - I have used my multimeter ( with care ) and determined that no power is getting to my side elements, and made sure power is coming into the kiln ok. Therefore you are correct that it is the relay that needs replacing. I will order one tomorrow, and am confident I can install, thanks so much for all the help.!!
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: kiln side elements not working

Post by Valerie Adams »

For a lack of power to one set of elements, I'd always replace relays first, since they're easy.
I had an extremely severe meltdown once, where the elements sagged out of the lid and were embedded in melted glass on the shelf. I cleaned them up, got them back into their groves, and continued to use that kiln without issue until I sold it.

Replacing relays are much easier than replacing elements!
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: kiln side elements not working

Post by Tony Smith »

Deb Brown wrote:Hi Arnold, Brad and Tony - I have used my multimeter ( with care ) and determined that no power is getting to my side elements, and made sure power is coming into the kiln ok. Therefore you are correct that it is the relay that needs replacing. I will order one tomorrow, and am confident I can install, thanks so much for all the help.!!
Please throw the circuit breaker and pull the plug before you do anything with the relays. The relays are always live when plugged in regardless of the switch position.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Deb Brown
Posts: 8
Joined: Tue Nov 19, 2013 10:42 am

Re: kiln side elements not working

Post by Deb Brown »

Thanks Tony. I have now successfully replaced my relay, and yayyyyy!!!!! my kiln is now working again. This solution is directly because of the input from this forum, I thank you all with all of my heart!!!
Post Reply