diamond glass tile saw blade size

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Val Eibner
Posts: 19
Joined: Thu Jan 08, 2004 2:01 pm
Location: BC, Canada
Contact:

diamond glass tile saw blade size

Post by Val Eibner »

Bought a 4" diamond blade at Lonnie's in Phoenix with a .012 kerf.
Seems pretty thin to cut fused glass pieces. Is there a better size kerf
to stick with instead of the .012. Have looked into the MK 303 4"
.20 Is that a better size? Thanks Val
Val
eibnerstudio
BC,Canada
Kevin Midgley
Posts: 773
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: diamond glass tile saw blade size

Post by Kevin Midgley »

Blade theory and practice.
Thinner wastes less glass per cut goes slower because of fewer diamonds.
Thicker can have more diamonds on the edge but will waste more glass.
Thinner can bend easier!
If you are doing pattern bars a regular tile saw with a 10" or bigger blade from HIS would be best.
If you want to get rid of the saw and blade and get a tile saw instead, PM me.
I am looking for a trim saw.
AndyT
Posts: 170
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: diamond glass tile saw blade size

Post by AndyT »

I bought a Ryobi 7" tile saw and a 7" glass tile blade. total cost about $150. Works great.
Kevin Midgley
Posts: 773
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: diamond glass tile saw blade size

Post by Kevin Midgley »

The larger the blade the longer potential blade life as they have more diamonds doing the work.
Smaller blades work and given the price of a large lapidary saw blade, you'd better be doing a lot of cutting to make it worth your while.
Val Eibner
Posts: 19
Joined: Thu Jan 08, 2004 2:01 pm
Location: BC, Canada
Contact:

Re: diamond glass tile saw blade size

Post by Val Eibner »

Thanks for the replies. I have a 7" tile saw already with good blade.
Wanted a small tile saw for straight cuts and some angles, but
convenient to set up and use in a pinch. Will probably take back the .012 kerf
blade and get a good .20 kerf from Rio Grande.
Val
eibnerstudio
BC,Canada
Tom Fuhrman
Posts: 187
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: diamond glass tile saw blade size

Post by Tom Fuhrman »

check out blades from www.lopacki.com, Dan used to have some good prices on the 4" diamond blades and he can be very helpful.
Post Reply