I want to do liquid screen printing, not the powder kind.  Where can I get glass paints in larger quantities than I find with Glassline paints?  I want to buy a pint/500ml of glass paint.
I'll even accept a good recipe for glass paint using a liquid media and pigments.
			
			
									
						
										
						Where can I get/make glass paints for screen printing?
Moderators: Brad Walker, Tony Smith
- 
				BillsBayou
 - Posts: 36
 - Joined: Wed Oct 29, 2014 1:08 pm
 
- 
				Kevin Midgley
 - Posts: 773
 - Joined: Mon Mar 10, 2003 11:36 am
 - Location: Tofino, British Columbia, Canada
 
Re: Where can I get/make glass paints for screen printing?
thompson enamels
			
			
									
						
										
						- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: Where can I get/make glass paints for screen printing?
Right from Warm Glass Studio's store  
http://www.warmglass.org/enamels
You can mix the medium in yourself. It's not hard to do.
			
			
									
						
							http://www.warmglass.org/enamels
You can mix the medium in yourself. It's not hard to do.
Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				Barry Kaiser
 - Posts: 311
 - Joined: Mon Jul 25, 2005 6:54 pm
 - Location: North Carolina
 - Contact:
 
Re: Where can I get/make glass paints for screen printing?
Kaiser Glass Paints....Made for screen printing
			
			
									
						
							Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
			
						http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
Re: Where can I get/make glass paints for screen printing?
I mixed Reusche's tracing black (and others - didn't seem to matter) with squeegee oil from Ulano, but I'd guess that there are many suppliers of screening media.
			
			
									
						