Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
Moderators: Brad Walker, Tony Smith
Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
I want to buy a circle cutter. I've never used one but it seems the Silbertschnitt (6 wheel) & Fletcher-Terry(3wheel) are good ones. I read a carbide head is available for the Fletcher is that true of the Silbertschnitt also.
Thank you,
Chris
Thank you,
Chris
-
Brad Walker
- Site Admin
- Posts: 1540
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
Get the Silberschnitt with the ball bearing head (not the turret). Mine is nearly 20 years old and still has original head despite heavy use.
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
Love my Fletcher_Terry have had it for many years
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
What Brad said. The Silberschnitt is the standard circle cutter across the commercial glass industry for a reason.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
You might also look far away online and find a 'well designed' circle cutter but you could wait a while for the delivery.
What you won't know about is the quality of the wheel or the thickness of the glass it was designed to cut.
From Asia, if you know your sources, a 'similar design of circle cutter' to those being discussed is $15 US plus maybe $5 postage and perhaps 3 weeks shipping.
Note I said similar.
Canadian source: http://www.hitechglazing.com/search
What you won't know about is the quality of the wheel or the thickness of the glass it was designed to cut.
From Asia, if you know your sources, a 'similar design of circle cutter' to those being discussed is $15 US plus maybe $5 postage and perhaps 3 weeks shipping.
Note I said similar.
Canadian source: http://www.hitechglazing.com/search
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
I love my Silberschnitt. I joke that every time I use it, I want to kiss a German (my husband is German
).
Dana W.
Dana W.
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
Silberschnitt truly is the Best!
....my rather prejudiced opinion ( yes, I am German!)
....my rather prejudiced opinion ( yes, I am German!)
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
The Silberschnitt with a single carbide wheel is good. The cheap one with the 6 wheel turret is horrible. Think about it. How do you know it is time to change wheels? That would be after a piece of glass breaks. Maybe cheap float glass guys can afford to lose some glass. Expensive glass cutting is a different story. Once you factor in the cost of 6 pieces of broken glass to the cost of your circle cutter, a carbide wheel cutter pays for itself.
I use the Toyo, and love it. http://www.fusionheadquarters.com/Toyo_ ... toycir.htm
Be careful, if you drop the cutting head on to the glass, the wheel will break. They are replaceable if you can see the tiny wheel and are dextrous enough to handle it. I've gotten good at it.
As to Fletcher cutters, the day I got control over glass cutting was the day I got my first Toyo carbide wheel cutter. I started out using Fletcher, both steel and carbide wheels. I have never turned back. I have been using Toyo cutters since the early 80's. I've tried some others but never like them.
I use the Toyo, and love it. http://www.fusionheadquarters.com/Toyo_ ... toycir.htm
Be careful, if you drop the cutting head on to the glass, the wheel will break. They are replaceable if you can see the tiny wheel and are dextrous enough to handle it. I've gotten good at it.
As to Fletcher cutters, the day I got control over glass cutting was the day I got my first Toyo carbide wheel cutter. I started out using Fletcher, both steel and carbide wheels. I have never turned back. I have been using Toyo cutters since the early 80's. I've tried some others but never like them.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
I love my turret head cutter
.
I will ask the same question back... with any cutter, how do you know it's time to change the wheel, other than you start having issues with cutting/breaking glass.
Dana W.
I will ask the same question back... with any cutter, how do you know it's time to change the wheel, other than you start having issues with cutting/breaking glass.
Dana W.
-
Brad Walker
- Site Admin
- Posts: 1540
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
That's how I know.JestersBaubles wrote:how do you know it's time to change the wheel, other than you start having issues with cutting/breaking glass.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
A steel wheel might be good for 10 or 20 circles. A Toyo or Silberschnitt carbide wheel might be good for 10 or 20 years.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Silbertschnitt vs Fletcher-Terry circle cutter - experiences?
I have cut many, many more than 20 circles with my Silberschnitt since I've had it. I am only on my second cutter head on the "turret".
Dana W.
Dana W.