I've been thinking about getting some UGC Accents in gold, bronze or platinum as I'd like some of these mettalic colours in my designs. But the supplier I can get them from doesn't state what glass COE they are compatible with (and haven't replied to my enquiry about it). I use Bullseye glass, so was wondering if anyone here has ever used them with BG, and if so do they give a nice mettalic effect or more of a matt effect.
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Has anyone used UGC Accents with Bullseye?
They should work with just about any glass that can be fired in the 1500F range. It's a thin enough layer that COE isn't really a significant issue.
Re: Has anyone used UGC Accents with Bullseye?
Thanks very much for your advice Brad. I'm excited to give this a go.