Best Glue for Garden Stakes

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Best Glue for Garden Stakes

Post by grammy »

I am replacing some glass for a client in their garden stakes. So these will be outside. The stakes do not have a way to "clip" in the glass, only glueing to the metal. What glue would be best? E6000?
Dick
Posts: 89
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: Best Glue for Garden Stakes

Post by Dick »

I don't trust e6000 as I have had some failures. Loctite h30cl hysol works great and stays crystal clear.
grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Re: Best Glue for Garden Stakes

Post by grammy »

Thank you.
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Best Glue for Garden Stakes

Post by DonMcClennen »

GE Silicone 2 will do the job well. I have outside installations now 15yrs old.... outside 4 seasons with NO failures!
"The Glassman"
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Best Glue for Garden Stakes

Post by Valerie Adams »

I'm with Don; silicone is my choice for outdoors.
grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Re: Best Glue for Garden Stakes

Post by grammy »

Thanks. I did not find the Loctite that was mentioned but got an epoxy for metal to glass.
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Best Glue for Garden Stakes

Post by Peter Angel »

DonMcClennen wrote:GE Silicone 2 will do the job well. I have outside installations now 15yrs old.... outside 4 seasons with NO failures!
Don, do you ever get mold growing on the cured silicone?

Pete
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Best Glue for Garden Stakes

Post by Buttercup »

Guess you can't replace it with grout, as we now have to do at all the floor/wall junctions in the showers. Damn! Jen
Post Reply