Best Glue for Garden Stakes
Moderators: Brad Walker, Tony Smith
Best Glue for Garden Stakes
I am replacing some glass for a client in their garden stakes. So these will be outside. The stakes do not have a way to "clip" in the glass, only glueing to the metal. What glue would be best? E6000?
Re: Best Glue for Garden Stakes
I don't trust e6000 as I have had some failures. Loctite h30cl hysol works great and stays crystal clear.
Re: Best Glue for Garden Stakes
Thank you.
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: Best Glue for Garden Stakes
GE Silicone 2 will do the job well. I have outside installations now 15yrs old.... outside 4 seasons with NO failures!
"The Glassman"
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Best Glue for Garden Stakes
I'm with Don; silicone is my choice for outdoors.
Re: Best Glue for Garden Stakes
Thanks. I did not find the Loctite that was mentioned but got an epoxy for metal to glass.
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: Best Glue for Garden Stakes
Don, do you ever get mold growing on the cured silicone?DonMcClennen wrote:GE Silicone 2 will do the job well. I have outside installations now 15yrs old.... outside 4 seasons with NO failures!
Pete
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Re: Best Glue for Garden Stakes
Guess you can't replace it with grout, as we now have to do at all the floor/wall junctions in the showers. Damn! Jen