Cutting 6mm slices on a tile saw

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
JeffP
Posts: 25
Joined: Fri Feb 22, 2013 8:51 am
Location: Queensland, Australia

Cutting 6mm slices on a tile saw

Post by JeffP »

Hi
Would really like to know how others are getting around a problem with most tile saws.
The problem is cutting 6mm slices from things like pattern bars.
Most saws have a wide slot in the table for the blade to run through. Cutting a 6mm slice has the danger that the slice will fall through the blade slot into the tray underneath or worse and hazardous, jam in the slot and damage the blade or me.
I have been told to buy a sheet of perspex and attach it to the table and then run the blade through it so it creates a narrow slot for the blade.
Problem, is how to attach it so it can be replaced when damaged, and it reduces the depth of cut.
Surely many of you do this and I would love to hear how you solved the problem.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Cutting 6mm slices on a tile saw

Post by Marty »

spring clamps
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Cutting 6mm slices on a tile saw

Post by Brad Walker »

I use a piece of 1/4"hardboard (pegboard, only without the holes). Don't attach to the table, just rest on top. Works well, and being 1/4" higher actually helps the blade cut better.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Cutting 6mm slices on a tile saw

Post by Marty »

Jeff- can't you adjust the blade height on your saw?
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Cutting 6mm slices on a tile saw

Post by Kevin Midgley »

scrap Styrofoam food packaging trays. Zero cost. Don't even have to cut the slot before cutting the glass.