Emissions and studio safety - WarmGlass.com

Emissions and studio safety

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
Geo
Posts: 48
Joined: Mon Jul 07, 2003 8:54 am

Emissions and studio safety

Postby Geo » Tue May 24, 2016 2:09 pm

The recent events has made me wonder about just what is happening to the air in my own studio if I'm fusing or casting with red colored glass, for instance. Any thoughts?

Brad Walker
Site Admin
Posts: 1385
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Emissions and studio safety

Postby Brad Walker » Tue May 24, 2016 2:21 pm

Geo wrote:The recent events has made me wonder about just what is happening to the air in my own studio if I'm fusing or casting with red colored glass, for instance. Any thoughts?


The problem occurs when the glass is being made, heated to 2400F or thereabouts, and some of the chemical components go up the smokestack and into the air. So long as you're just fusing or casting, no issue, any potentially hazardous chemicals are not released.

Marty
Posts: 855
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Emissions and studio safety

Postby Marty » Tue May 24, 2016 9:29 pm

But there's binders in the refractories that burn off, dusts from working with powders and from sandblasting, mists from coldworking. Common sense ventilation takes care of most, particle masks the rest.

Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Emissions and studio safety

Postby Greg Rawls » Wed May 25, 2016 7:00 am

Greg


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 60 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com