To what extent do low spots in kiln shelves contribute to the development of fused glass bubbles? I am checking a flat-ground shelf with a steel ruler and wondered what you thought.

Thanks,

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com
Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: Kiln shelves ground flat

Post by Rick Wilton »

in a word...... Hugely.
Rick Wilton
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Kiln shelves ground flat

Post by Kevin Midgley »

there are however, no guarantees that a flat shelf will over time remain flat......
A lot depends of how it is used and or abused by that use.
Large thermal masses in one location or support of lack of support can possibly cause changes.

Nobody will knowingly sell as new, warped kiln shelves so to get the bubble forming dips people complain about takes firing time in a kiln.