Just a thought.
I have a small ultrasonic cleaner left from when I was doing jewelry, and decided to give it a try.
I put some h2o in three bottles and fired that sucker up.
After about 1 hour the paint in the bottles had all reconstituted itself.
NOW, for the TE pens.
I unscrewed the tip and put some h2o in and put them in with the Glassline paints, and Viola,. the same thing.
I just saved about $400.00 for nothing.
NOTE VERY IMPORTANT. My TE pens were about 10 years old, so this might not be applicable now.
The threads are LEFT HANDED!!!!
Dried up
Moderators: Brad Walker, Tony Smith
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Dried up
GREAT idea Jim. Now to find a cheap ultrasonic cleaner with longer than a 90 second timer or running on the 'wrong' voltage. 