Post by Havi »

Hello everybody!
Can I make glue, for glass, mixing methyl cellulose with water??? [Actually I am seeking a way to create something like gel i.e. thicker than regular liquid glue]

Or

Does it have to be mixing CMC with water???
Of course, with the right proportions.

Many thanks in advance,

Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: METHYL CELLULOSE or CMC

Post by Brad Walker »

Easy to do. Here are the instructions: http://richardlalonde.com/liquid-glass-line-updated/
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: METHYL CELLULOSE or CMC

Post by Havi »

Thank you "know All" Brad!!



Just copied to my notebook LaLonde's instructions.
However, I am asking if it is possible to make a thickened glue NOT from CMC but from METHYL CELLULOSE.... Is it the same, or different?

Many thanks,

Havi
ps look for a pm from me
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: METHYL CELLULOSE or CMC

Post by Brad Walker »

CMC is carboxyl methyl cellulose. Methyl Cellulose is chemically a bit different, but has many of the same properties. But since both are used as food thickeners and as glues, I would give it a try using Richard's procedure. I'd be surprised if it didn't work.

Remember -- make it up a little thicker than the recipe. You can always dilute later, but you can't thicken it after it's been made.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: METHYL CELLULOSE or CMC

Post by Havi »

Thanks!

H.
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: METHYL CELLULOSE or CMC

Post by Havi »

Just an update.
I did some textures with. Methyl cellulose - it works very well for me!

Thanks again for the advise, Brad.

as always - this is really the best place for good relyable information

H
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)