Silver Sand for Sandmold
Moderator: Tony Smith
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Silver Sand for Sandmold
Hello ! Is it possible to use Silver Sand for making a Sandmold (sand and Aluminium Hydrate) ? Jan
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Silver Sand for Sandmold
Difficult question, or did I give to little information ? greetings from Holland, Jan
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Silver Sand for Sandmold
What is "silver sand?"
You might want to look up the melting point of Al.
Jim
You might want to look up the melting point of Al.
Jim
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: Silver Sand for Sandmold
I'm not familiar with the term "silver sand", but Bert is probably the best resource for your question. He introduced me to alumina hydrate years ago.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Silver Sand for Sandmold
Yes, now I understand the problem: did translate the Dutch word, but now I realise it is bad translation 
Zilverzand (Dutch) = Quartz sand , silica sand or white sand is fine-grained, white, extremely pure sand with low iron content . It consists almost entirely of quartz (SiO 2 ) Now I know it is full of quartz I know the use in the kiln is not good, so I will going use Olivinesand. Thank you ! Jan
Zilverzand (Dutch) = Quartz sand , silica sand or white sand is fine-grained, white, extremely pure sand with low iron content . It consists almost entirely of quartz (SiO 2 ) Now I know it is full of quartz I know the use in the kiln is not good, so I will going use Olivinesand. Thank you ! Jan