Hello ! Is it possible to use Silver Sand for making a Sandmold (sand and Aluminium Hydrate) ? Jan
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Silver Sand for Sandmold

Post by Jan de Jong »

Difficult question, or did I give to little information ? greetings from Holland, Jan
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Silver Sand for Sandmold

Post by jim simmons »

What is "silver sand?"
You might want to look up the melting point of Al.
Jim
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Silver Sand for Sandmold

Post by Tony Smith »

I'm not familiar with the term "silver sand", but Bert is probably the best resource for your question. He introduced me to alumina hydrate years ago.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Silver Sand for Sandmold

Post by Jan de Jong »

Yes, now I understand the problem: did translate the Dutch word, but now I realise it is bad translation :)
Zilverzand (Dutch) = Quartz sand , silica sand or white sand is fine-grained, white, extremely pure sand with low iron content . It consists almost entirely of quartz (SiO 2 ) Now I know it is full of quartz I know the use in the kiln is not good, so I will going use Olivinesand. Thank you ! Jan