Annealing Question

Post by grammy »

I am getting back into fusing glass. I have some small jewelry sized piesces that are double thick fully fused. I am now adding a decal to these pieces. These are low heat 24kt gold decals that say go to 1100. Do I have to anneal these? Just wondering if I can get by without it.

Thanks
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Annealing Question

Post by jim simmons »

I would, just to be on the safe side
You do not want a customer to have one brealk.
Why not? It doesn't take all that long.
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Annealing Question

Post by Barry Kaiser »

Go a little higher, say 1200. no need to hold.
When cooling, just turn it off. you will be fine.
I refire 6mm pieces and crash to 900, then recover,crash a second time, and open the kiln at about 500 (top loading kiln, mulllite shelves...makes a difference.)

Barry
Kevin Midgley
Posts: 773
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Annealing Question

Post by Kevin Midgley »

Always anneal.