Coldworking/grinding leaded crystal?...

Postby Mia M » Sun Jan 08, 2017 1:16 am

Unfortunately, grinding the mold lines for my leaded crystal sculptures is a necessity, so it can't be avoided. My only choice seems to be to grind in a booth with an exhaust fan, wear a mask, and be as careful as possible. Any thoughts about leaded crystal coldworking and safety?...
Last edited by Mia M on Sun Feb 19, 2017 7:18 pm, edited 1 time in total.

jolly
Posts: 61
Joined: Thu Jan 08, 2004 7:44 pm
Location: Port Townsend, WA

Re: Coldworking/grinding leaded crystal?...

Postby jolly » Thu Jan 12, 2017 9:35 am

I don't consider any glass dust to be safe for exposure to my lungs so I certainly wouldn't consider leaded glass to be safe. If it were me, I would use the same precautions as for any grinding of glass and then I would buy a lead testing kit -the EPA has some recommendation on which kits are best- and test the slurry to see if the lead is now a problem for disposal.
There is more to life than increasing its speed.-Mahatma Gandhi

Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Coldworking/grinding leaded crystal?...

Postby Greg Rawls » Fri Jan 13, 2017 8:19 am

There are a lot of variables here - how much available lead in the crystal, how much and how long you are grinding, how you are grinding, etc. My recommendation is to grind wet and wear a P100 respirator. Try to contain the dust and carefully clean your equipment when finished.

Greg, retired Certified Industrial Hygienist
Greg

Mia M
Posts: 5
Joined: Sat Jan 07, 2017 11:32 pm

Re: Coldworking/grinding leaded crystal?...

Postby Mia M » Sun Feb 19, 2017 7:15 pm

Thank you, Jolly and Greg. I appreciate your comments and will try to follow your suggestions.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 7 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com