metalic stains after blasting

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

metalic stains after blasting

Post by peter cummings »

Kiln is rewired, experiments starting.
I've noticed that after sandblasting, the glass is susceptible to staining, from lots of things, some of it seems permanent even without firing.
Thinking of trying copper sulphate, that puts greenish tinge on bronze castings, or rust in a solvent of some type. Using float.
Any clues, references welcome. As usual I'm happy to share anything I find out.
Thanks. Peter.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: metalic stains after blasting

Post by Brad Walker »

Alex Bernstein fuses steel to the surfaces of his cast glass: http://alexbernsteinglass.com/artwork/ He makes some really fascinating sculptures.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: metalic stains after blasting

Post by Kevin Midgley »

essentially any oil based paint will stick in the pores of the blasting.
If you buff and then repeat buff and repeat, you can build up a finish.
Done often enough you have the paint forming a solid film and colour.
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

Re: metalic stains after blasting

Post by peter cummings »

Thanks Brad and Kevin. That is some studio Alex has, and looks interesting works. I can't get right into the pictures though, either website or flickr problem. I'll try the paint as Kevin suggested, maybe like my recent wood stain effort, painters oil paint mixed with gum turps, apply and wipe back. It's an organic Galle look I'm after.
I'll let you know, and it's good to catch up again.
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: metalic stains after blasting

Post by Tony Smith »

Peter,

Check out Sculpt Nouveau. http://www.sculptnouveau.com

They have a YouTube page as well.

They have patinas and base finishes for all materials that replicate many different oxides.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

Re: metalic stains after blasting

Post by peter cummings »

Thanks Tony. Beautiful colours and finishes. I see they "road freight" and I've sent email questions. I'll also look for metal finishes over here.
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

Re: metalic stains after blasting

Post by peter cummings »

Yah Tony. Sculptnouveau have a distributor in Australia, that has opened a new store in Melbourne. My capital. They tell me some of their products will work on glass. A trip to town coming up.
Peter.
Post Reply