Hello !   Please can anybody give me a schedule for firing and slumping a bowl of Car window Glass (I hope I use the right words in English for this material 
  ) Thank you, Jan from Holland
			
			
									
						
										
						- 
				DonMcClennen
 - Posts: 381
 - Joined: Sun Mar 09, 2003 9:09 pm
 - Location: Ontario
 
Re: Car window glass
Car window glass use to be 2 thin layers of a glass sandwich with a thin plastic layer in the middle. If this is still the way its made then fusing is not an option..
			
			
									
						
							"The Glassman"
			
						- 
				Rick Wilton
 - Posts: 273
 - Joined: Sat Oct 25, 2003 8:18 pm
 - Location: Calgary, Canada
 - Contact:
 
Re: Car window glass
Car WINDOWS are tempered....... car windshields are laminated.
Windows good to fuse
Windshields NOPE
			
			
									
						
							Windows good to fuse
Windshields NOPE
Rick Wilton
			
						- 
				Jan de Jong
 - Posts: 114
 - Joined: Sun Mar 09, 2003 3:31 pm
 - Location: The Netherlands
 
Re: Car window glass
Thank you for your answer and sorry for the late response (waiting on a mail that there was a post, but that was in the paste !) But do you have a schedule for fusing and slumping this glass (or is that the same as "normal" window glass) ?? Jan de Jong (from Holland)Rick Wilton wrote:Car WINDOWS are tempered....... car windshields are laminated.
Windows good to fuse
Windshields NOPE