Post by susanmozingo »

How can you tell which side is the top side of a clear sheet of System 96?
AndyT
Posts: 170
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Spectrum System 96

Post by AndyT »

susanmozingo wrote:How can you tell which side is the top side of a clear sheet of System 96?
If you have any seeds in it they are on the bottom. also, the back side usually has a slight matte look.
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Spectrum System 96

Post by JestersBaubles »

I don't think there is really a "top" side. There is a smooth side and a side that is a bit textured. Depending upon what you are doing dictates which side is facing up.

For instance, when layering glass pieces, I will try to put texture facing texture, or at least texture facing smooth to minimize bubbles (smooth to smooth is when you'll more likely get bubbles).

Best, Dana
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Spectrum System 96

Post by Tony Smith »

Jim is right, but keep in mind that art glass isn't like float glass which has one side "contaminated" by the float process.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Spectrum System 96

Post by jim simmons »

Tony.
By "contamination" I assume that you mean the tin left by the float process.
The other Jim
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Spectrum System 96

Post by Tony Smith »

jim simmons wrote:Tony.
By "contamination" I assume that you mean the tin left by the float process.
The other Jim
Yup. That's what I meant, and why most people ask which side is up.

Tony