I would like to know how to eliminate/minimize a break.
I have a piece of BE that broke and I still want to use to make a bowl.
Should the break be put on the top or the bottom of the 2 layer stack for the fusing?
Thanks
The other Jim
healing a broken piece of glas.
Moderator: Tony Smith
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: healing a broken piece of glas.
The bottom.