Making a rainbow
Moderator: Tony Smith
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Making a rainbow
Hello ! Is there a simple way to make a "rainbow" (half-circle) with 6-7 colours ? Jan de Jong
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Making a rainbow
Sure.
cut a circle then cut it in half and layer different frits on it.
The other Jim
cut a circle then cut it in half and layer different frits on it.
The other Jim
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Making a rainbow
Thank you Jim ! Is there a way to do it with sheet glass (as I still did not work with frits and not have them). Is it possible with a saw ? Janjim simmons wrote:Sure.
cut a circle then cut it in half and layer different frits on it.
The other Jim
-
Fiona Collins
- Posts: 30
- Joined: Sun Nov 17, 2013 9:10 am
Re: Making a rainbow
Cut a half sheet of clear and butt against 1/2 sheet of first colour. Place your circle cutter in the middle of the join, score half circle on the colour sheet, adust length in 15mm, leave base as is, run second score. Replace colour sheet with second colour, score with same setting as previous, adjust length in 15mm ... rinse and repeat 4 times. Carefully run and break out each segment
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Making a rainbow
@ Fiona Collins: Thank you ! Jan