I have a bunch of cut circles and would like o know how to calculate the maximum square in a given circle.
Any suggestions?
Thanks
The other Jim
squares iout of circles
Moderator: Tony Smith
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: squares iout of circles
Back to basic geometry!
D squared divided by 2 equals S squared.
Where D is the diameter of the circle and S is the side of the maximum square.
D squared divided by 2 equals S squared.
Where D is the diameter of the circle and S is the side of the maximum square.
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: squares iout of circles
Jim,
Its 0.707 x diameter
So if you have a 10" diameter, 10" is the hypotenuse or long side of the square
Pythagorean theorem says the square of the hypotenuse of a right triangle equals the sum of the squares of the other sides so,
a^2 + b^2 = c^2
c=10, so 10 ^2 = 100
Since a square has equal sides, a = b so we can write the equation as
2 a^2 = 100
Dividing both sides by 2 we get
a^2 = 50
Take the square root of both sides giving you
a = sqrt 50 = 7.07
So for a 10" diameter, you can fit a 7.07" square. For any other diameter, you can just multiply 0.707 x diameter
I hope this helps
Tony
Its 0.707 x diameter
So if you have a 10" diameter, 10" is the hypotenuse or long side of the square
Pythagorean theorem says the square of the hypotenuse of a right triangle equals the sum of the squares of the other sides so,
a^2 + b^2 = c^2
c=10, so 10 ^2 = 100
Since a square has equal sides, a = b so we can write the equation as
2 a^2 = 100
Dividing both sides by 2 we get
a^2 = 50
Take the square root of both sides giving you
a = sqrt 50 = 7.07
So for a 10" diameter, you can fit a 7.07" square. For any other diameter, you can just multiply 0.707 x diameter
I hope this helps
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: squares iout of circles
.....and then after all those careful calculations there is the flow of the glass to consider.
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: squares iout of circles
Thanks you all, ESPECIALLY Tony.
The other Jim
The other Jim
Re: squares iout of circles
I just divide the circle in half both ways and then connect the ends of each line to the one next to it.
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact: