I just got back from Glass Craft Expo. There was some great stuff. I got to take a lot of classes including a pate de verre class stack block class, a Bullseye box casting demo. Came back loaded to the gills with glass and tools & lots of great products.
I brought back some of Armstrong's new patterned & colored float compatible glass as well as Youghiogheny's colored transparent float compatible.
I have not done much with float but am hoping this glass will be fun.
Has anyone here tried it?
I brought back some of Armstrong's new patterned & colored float compatible glass as well as Youghiogheny's colored transparent float compatible.
I have not done much with float but am hoping this glass will be fun.
Has anyone here tried it?
-
Dennis Brady
- Posts: 64
- Joined: Fri Dec 19, 2003 9:06 pm
- Location: Victoria BC
- Contact:
Haven't tried the Yucky but the Armstrong is terrific. Especially if you want to fire large pieces (like door lites). My ONLY complaint is there's so far a very restricted colour palette but I'm hoping that will soon be expanded. Having glass that can be fused onto large door lites and full size windows (6 to 8 ft tall) opens up many new opportunities for architectural applications.
Was that not a terrific show? When we were packing out after, there were people lined up to register early for classes next year. We've already booked a bigger exhibit booth and planning extra classes for 2005.
Was that not a terrific show? When we were packing out after, there were people lined up to register early for classes next year. We've already booked a bigger exhibit booth and planning extra classes for 2005.
DeBrady Glass Ltd http://www.debrady.com
Victorian Art Glass http://www.vicartglass.com
Glass Campus online classes http://www.glasscampus.com
Victorian Art Glass http://www.vicartglass.com
Glass Campus online classes http://www.glasscampus.com
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Rosannarosanna gusler wrote:so is this glass the same that is on their website? sort of a mottled enameled looking glass? rosanna
I saw the Armstrong glass when I was in Portland. I was astounded at what garbage it was. It is enamel smeared on thin float glass. A total waste of glass and enamel to my eye. First of all, I often find thin and thicker float glasses incompatible. Second of all, The smeared enamels were ugly, poor imitations of stained glass.
I am curious about Yough's transparent colors. I wonder if they are more vibrant than Thompson's or lower melting temp than the CR LOO frits. I am more interested in the frits made from them than I am in using sheets. Thompson made wonderful colors before they took the lead out and killed the colors. Transparency is still an elusive factor for me with the exception of blue.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
It is enamel on glass but I actually liked it. I am not sure it was meant tp look like stained glass, I think it has a distinct look that has lots of possibilities.I saw the Armstrong glass when I was in Portland. I was astounded at what garbage it was. It is enamel smeared on thin float glass. A total waste of glass and enamel to my eye.
The Youghiogheny colors are really pretty. There is a Violet, a Kelly Green, a light blue & an Erbium Pink.
-
Lynne Chappell
- Posts: 186
- Joined: Fri Mar 14, 2003 2:05 am
- Location: Surrey B.C. Canada
- Contact:
Enamels on glass are "generally" more like Oil Paints, not like Stained glass. If you want that depth of color, get colored glass.
Youghigheny (sp) flat glass. Anyone have an address? I probably could/should search, but I'm typing right now. And the spelling would cause me much trial, even though , as a child, I went to Ohiopyle annually.
Greg
Youghigheny (sp) flat glass. Anyone have an address? I probably could/should search, but I'm typing right now. And the spelling would cause me much trial, even though , as a child, I went to Ohiopyle annually.
Greg
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Forgot the "o": http://www.youghioghenyglass.com/watershed wrote:Youghigheny (sp) flat glass. Anyone have an address?