Hi, we lived abroad for 7 years and I am just now returning to glasswork. My equipment and supplies were in a storage facility without heat or a/c. I fired my first pieces and they all migrated to the middle of the kiln shelf and fused together. I used the Basic 6 schedule from this site BASIC 6-Segment Firing Schedules.
http://system96.com/Resources/FiringGuideFahrenheit.pdf with System 96 glass. I suspect the temp was too high but fear there might be other contributing factors.
I used Thinfire shelf paper that no longer looks white from being in storage so long. It looks beige. Does shelf paper deteriorate?
I used to fire my kilns in my kitchen but have room in the garage in our new house. It was colder (low of 40 F0 and rainy when I fired. Does the garage need to be heated?
Thanks in advance for your kind assistance.
Diane
Help with disaster fire
Moderators: Brad Walker, Tony Smith
Help with disaster fire
- Attachments
-
- FullSizeRender.jpg (31.33 KiB) Viewed 165622 times
-
The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: Help with disaster fire
The old version of thinfire would shrink and curl up. Which may be the cause of your problem since your pieces are small.
Jim "The Hobbyist"
Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Re: Help with disaster fire
Is there a chance your shelf was stored in such a way that may have allowed it to warp slightly?
Vonon
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Help with disaster fire
Also, you might want to weigh down the edges/corners with some kind of kiln furniture.
This will keep it from curling so much.
The other Jim
This will keep it from curling so much.
The other Jim
Re: Help with disaster fire
Thanks JIM. I will check my self. The kiln furniture is a great idea!
Re: Help with disaster fire
Dang spellcheck. Shelf!
-
Ed Cantarella
- Posts: 155
- Joined: Mon Feb 26, 2018 3:49 pm
- Location: Highland, Michigan, USA
Re: Help with disaster fire
At least it wasn't elf.dianes wrote:Dang spellcheck. Shelf!
BOT - what a drag.
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.