Post by cbrandt »

Is it possible to fire polish the bottom of a platter that is already slumped without losing its shape? I've already tried repeating my regular slumping schedule with it on the mold resulting in a small part now slightly shiny and the rest still matte from previous sandblasting. I can increase the temperature but wonder what if any temperature will work if it's not going to make any difference because it's on the mold.
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Polishing bottom of slumped platter

Post by Brad Walker »

The only part of glass that will shine during a firing are parts that are exposed to air during the firing. So the bottom of a slumped piece won't shine up during the firing.

There are some products that claim to shine up the bottom at lower temperatures, but most don't really result in a shine, just a changed appearance.
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Polishing bottom of slumped platter

Post by jim simmons »

The only way that I know of, would be to cold work the bottom working all the way up tp a 1400 grit.