HI All,
I have a water scene that I have already fired, B.E. .clear,with frits size is 12 x 6 Now I want to put that on top of B.E. 4200
do I add more soak time and ramp up slower?
Thanks, Tracey
firing schedule
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: firing schedule
Yes, absolutely. Slower up and longer anneal on the way down.
Also, don't forget that the second firing will cause any tack fused items to become more fused.
Also, don't forget that the second firing will cause any tack fused items to become more fused.