Hello friends,
during a fusing the window of my paragin sc2 with door and window become black and i am not able to see inside anymore?
what do you think happened?..and any way to restore the glass to look again inside?
thanks for support and collaboration,
mike
paragon window
Moderators: Brad Walker, Tony Smith
-
mikefromitaly
- Posts: 67
- Joined: Thu Apr 03, 2003 7:47 am
- Location: italy-sicily
- Contact:
paragon window
thanks for sharing !
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly
-
Joyce Walters
- Posts: 80
- Joined: Thu Nov 08, 2007 12:06 am
- Location: Stevensville MT
Re: paragon window
Hi Mike.
Do you know what caught on fire in the kiln?
Maybe it was just smoke from the kiln paper not vented?
Joyce from MT
Do you know what caught on fire in the kiln?
Maybe it was just smoke from the kiln paper not vented?
Joyce from MT
-
Ed Cantarella
- Posts: 155
- Joined: Mon Feb 26, 2018 3:49 pm
- Location: Highland, Michigan, USA
Re: paragon window
After trying to clean it, maybe try a little cerium oxide with a wet cloth. To polish the surface. Hopefully it is not ruined. 
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.
-
mikefromitaly
- Posts: 67
- Joined: Thu Apr 03, 2003 7:47 am
- Location: italy-sicily
- Contact:
Re: paragon window
Hi
Thank you.
I used thinfire paper of bullseye..and you are right.. Maybe was the fumes not vented.
It was not easy to clean but i did in the end.
So in which case i have to vent the kiln? And how?
(My paragon has a cone on the top?)
Thanks for your support and collaboration
Mike
Thank you.
I used thinfire paper of bullseye..and you are right.. Maybe was the fumes not vented.
It was not easy to clean but i did in the end.
So in which case i have to vent the kiln? And how?
(My paragon has a cone on the top?)
Thanks for your support and collaboration
Mike
thanks for sharing !
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly