Post by kgordon »

I am making a kitchenette in our basement - including a cement table top and having professionals fabricate the counters. Has anyone had any experience with using fused glass elements embedded into the concrete -like any inlay (not the recycled glass bits as you see everywhere). Thanks for any advice. Kim
SC19881
Posts: 1
Joined: Wed Feb 02, 2011 2:08 pm

Re: using embedded fused glass in cement countertop

Post by SC19881 »

Hi Kim
I have just finished casting and staining a cement table top with a 12 x 12 fused glass textured greenman tile inset into the cement.

I used the reversed process of casting this (table top was on the bottom of the form. The tile appears to be very well set in the cement.

HTH,