Playing with Color Bars and Vitrigraph

Want to share a photo of your work? Or get feedback on a new piece? Post it here. (Note: items in this forum are deleted periodically, generally after several months.)

Moderator: Brad Walker

Post Reply
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Playing with Color Bars and Vitrigraph

Post by twin vision glass »

I have been having fun slicing and chopping and creating with color bars and vitrigraph.
php2KGdH9PM.jpg
php2KGdH9PM.jpg (52.52 KiB) Viewed 32410 times
phpqmiAuzPM.jpg
phpqmiAuzPM.jpg (46.97 KiB) Viewed 32410 times
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Playing with Color Bars and Vitrigraph

Post by Kevin Midgley »

Crazy amount of work in there! Wow.
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Playing with Color Bars and Vitrigraph

Post by twin vision glass »

phpZzbPrEPM.jpg
phpZzbPrEPM.jpg (49.27 KiB) Viewed 32402 times
How are you Kevin. Here is the ground being created.
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
FusedLightStudio
Posts: 58
Joined: Wed Jan 24, 2018 1:33 pm
Location: Georgia
Contact:

Re: Playing with Color Bars and Vitrigraph

Post by FusedLightStudio »

Fantastic! And very inspiring. Thanks for posting!
Lisa Schnellinger
Atlanta, GA
twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: Playing with Color Bars and Vitrigraph

Post by twin vision glass »

phpbpwu4zAM.jpg
phpbpwu4zAM.jpg (50.48 KiB) Viewed 32365 times
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com