firing schedule

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
raphy
Posts: 27
Joined: Sun Jul 02, 2006 8:22 pm
Location: los angeles

firing schedule

Post by raphy »

mine: for three layer 71/2 x 11 assembled frit sheets. which works

300 1215 2.00
100 1490 :20
9999 910 2:00
100 750 .15
However I am now doing four layers of 12x12 assembled frit sheets. Do you think I need to change this schedule at all. Thank you for any advice, I'm really bad at changing schedules that I know work.
The Hobbyist
Posts: 309
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: firing schedule

Post by The Hobbyist »

I would add/change 50 800 to the anneal for this one and the next.