Question about ceramic rope
Hello! When I use 1 - 1,5 mm ceramic rope between 4 layers of glass Full fuse, will it become brittle or can I use it later for another lower temp fusing ? Jan
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Question about ceramic rope
Could you please explain what you are trying to do?
That would help a lot
The other Jim
That would help a lot
The other Jim
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Question about ceramic rope
Hello ! I will try to explain. I want to make a necklace of cubics 1 x 1 x 1 cm , where the height will be a little more, as I take 4 layers of transparent glass.
For the holes I had the idea a 1 - 1,5 mm ceramic rope, using it the whole length for as many cubics as I can place on my kiln-plate. Full fuse them. Then I have to get a shiny gloss on ALL the sides. Is the rope still strong enough to hang it with the cubics between kiln stands to fire again ?? Sorry, more and more difficult for me to find the right words in English.
I hope it is clear. Jan de Jong
For the holes I had the idea a 1 - 1,5 mm ceramic rope, using it the whole length for as many cubics as I can place on my kiln-plate. Full fuse them. Then I have to get a shiny gloss on ALL the sides. Is the rope still strong enough to hang it with the cubics between kiln stands to fire again ?? Sorry, more and more difficult for me to find the right words in English.
I hope it is clear. Jan de Jong
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Question about ceramic rope
use a kiln wash coated stainless steel welding rod. I don't think rope will hold up the weight.
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Question about ceramic rope
You can find the rods at any welding supply store.
The other Jim
The other Jim
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Question about ceramic rope
@ Kevin + Jim: Thank you both !! Jan de Jong