Question about ceramic rope

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Question about ceramic rope

Post by Jan de Jong »

Hello! When I use 1 - 1,5 mm ceramic rope between 4 layers of glass Full fuse, will it become brittle or can I use it later for another lower temp fusing ? Jan
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Question about ceramic rope

Post by jim simmons »

Could you please explain what you are trying to do?
That would help a lot
The other Jim
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Question about ceramic rope

Post by Jan de Jong »

Hello ! I will try to explain. I want to make a necklace of cubics 1 x 1 x 1 cm , where the height will be a little more, as I take 4 layers of transparent glass.
For the holes I had the idea a 1 - 1,5 mm ceramic rope, using it the whole length for as many cubics as I can place on my kiln-plate. Full fuse them. Then I have to get a shiny gloss on ALL the sides. Is the rope still strong enough to hang it with the cubics between kiln stands to fire again ?? Sorry, more and more difficult for me to find the right words in English.
I hope it is clear. Jan de Jong
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Question about ceramic rope

Post by Kevin Midgley »

use a kiln wash coated stainless steel welding rod. I don't think rope will hold up the weight.
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Question about ceramic rope

Post by Jan de Jong »

@ Kevin + Jim: Thank you both !! Jan de Jong