coldworking disc grinder

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

coldworking disc grinder

Post by mikefromitaly »

Hello people
i am interested in purchasing a disc grinder to use with different grits until to polish with pumice and/or cerium

What about your experience to suggest me a good tool?

thanks for support and collaboration

mike
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

http://www.picturetrail.com/mikefromitaly
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: coldworking disc grinder

Post by Marty »

Talk to the stone workers near you. Glass is close enough to granite in hardness. You want the tools that everyone else is using (for supplies and repairs).
Post Reply