Wetbelt sander belts breaking

Post by Greg Rawls »

I have a bunch of belts for my wetbelt sander that are a few years old that are splitting at the seam after a few minutes of use. Consistently! Does the glue that holds the belt together have a shelf life? Anyone else had this problem?
Greg
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Wetbelt sander belts breaking

Post by Brad Walker »

Funny you mention this, Greg. I had two split on me just a couple of weeks ago. Don't know why. The belts were purchased several years ago, so perhaps there's a shelf life issue. But I've never had the problem before.
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Wetbelt sander belts breaking

Post by Tony Smith »

Are these full-size belts or Covington size? I've never heard of belts coming apart, but I suppose it's possible as the glue hardens over time.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Wetbelt sander belts breaking

Post by Brad Walker »

Tony Smith wrote:Are these full-size belts or Covington size? I've never heard of belts coming apart, but I suppose it's possible as the glue hardens over time.
Full-size. I'd never heard of it either until it happened twice this past month.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Wetbelt sander belts breaking

Post by Marty »

I've never had one split either. Mine fray.
I have to change some out and the new ones are several years old. Stay tuned.
Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Wetbelt sander belts breaking

Post by Greg Rawls »

These belts are 41-1/2 x 3. One belt breaking would not be an issue, but every time I replace the belt from my old stash (and these are maybe 4-6 years old), they work for a few minutes then split right at the seam.
Greg
FusedLightStudio
Posts: 58
Joined: Wed Jan 24, 2018 1:33 pm
Location: Georgia
Contact:

Re: Wetbelt sander belts breaking

Post by FusedLightStudio »

Greg Rawls wrote:These belts are 41-1/2 x 3. One belt breaking would not be an issue, but every time I replace the belt from my old stash (and these are maybe 4-6 years old), they work for a few minutes then split right at the seam.
Yep. Same exact problem. Had to buy new belts. But I cut up the old belts into small pieces to use as wet sandpaper for curves.
Lisa Schnellinger
Atlanta, GA
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Wetbelt sander belts breaking

Post by Marty »

Marty wrote:I've never had one split either. Mine fray.
I have to change some out and the new ones are several years old. Stay tuned.
Full sized belts, from HIS.
Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Wetbelt sander belts breaking

Post by Greg Rawls »

FusedLightStudio wrote:
Greg Rawls wrote:These belts are 41-1/2 x 3. One belt breaking would not be an issue, but every time I replace the belt from my old stash (and these are maybe 4-6 years old), they work for a few minutes then split right at the seam.
Yep. Same exact problem. Had to buy new belts. But I cut up the old belts into small pieces to use as wet sandpaper for curves.
That is a REALLY GOOD IDEA! Thanks!
Greg
Marian
Posts: 71
Joined: Mon Dec 06, 2004 5:37 pm
Location: Big Island Hawaii
Contact:

Re: Wetbelt sander belts breaking

Post by Marian »

I had that happen with a batch of belts also, from CRL. They work for 15 minutes and then let go. They were a few years old when I got around to needing them. It was only one size that broke. I bought new different ones from HIS.
ejgiebel
Posts: 11
Joined: Mon May 11, 2009 7:50 pm

Re: Wetbelt sander belts breaking

Post by ejgiebel »

Bit delayed in my response, but I saw a YouTube video on this a while back. Get some seam tape (not actually tape, but the fabric material they use to strengthen clothing seams) from a fabric store. Cut the seam tape to the width of the belt, one layer thick (seems to me it's folded over on itself, so you just want one layer). Scrape off the old seam material with a razor blade. Place the ends of the belt grit side down on a piece of wax paper (so the glue won't stick to it if it seeps through the seam), firmly hold the belt in place with the seam matching. Spread a thin layer of Gorilla Glue (it's water proof, super glue is not) on the belt. You want enough to hold, but don't get wild and crazy since the Gorilla Glue expands and can push through the seam onto the grit. Place the seam tape in the glue, add a bit more glue to saturate the tape. Spread the glue flat, place a weight (again, use wax paper because Gorilla Glue really sticks) over the seam and let dry (I think 24 hours is their recommend full cure time). You can make the piece of tape slightly larger than the belt and trim it once the glue dries (but the glue will be hard).

I repaired a belt that lasted about 30 minutes when new 2 years ago (OK, don't use the belt a lot, but I've used it 10 hours since then) and it is still holding strong.

Ed