Mica in Casting Mold

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Terry Gallentine
Posts: 195
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Mica in Casting Mold

Post by Terry Gallentine »

Has anyone out there tried putting a thin coating of mica on the surfaces of a casting mold for a pot casting? Mainly I am curious as to whether the mica will move with the flowing glass or will it form a fairly uniform outer coating.
Kevin Midgley
Posts: 773
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Mica in Casting Mold

Post by Kevin Midgley »

I found that with a mold containing mica in the mold matrix that the mica left marks in the glass.