Round piece of glass.....sagging

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Round piece of glass.....sagging

Post by Jan de Jong »

Hello ! I have no idea what will happen when you let sagg a round piece of glass. Is there anywhere a photo of this ?? Thank you, Jan de Jong
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Round piece of glass.....sagging

Post by Jan de Jong »

@ Jim Simmons: 26 cm diameter over kilnstands with on the top ceramic thick paper (felt ?). As I did for tealights but then square and not so big. Jan
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Round piece of glass.....sagging

Post by The Hobbyist »

The circle will sag like the square, by folding in a few places. If centered on the post it will end up with even height edges without the peaks you get with a square drape/sag.

Do a test with a circle of float to see if you get the effect you want.

Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Round piece of glass.....sagging

Post by Jan de Jong »

@ The Hobbyist: Thank you ! I will do a test. Jan de Jong
Post Reply