https://www.youtube.com/watch?v=le96sNV_b0Y&t=28s
MM6
Moderators: Brad Walker, Tony Smith
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
MM6
There was a discussion awhile ago about Zircar Luminar MM6 . Many were wanting to know how to use it so I decided to try to help out by working with Zircar and doing a video and some PDF s for them. They have posted the video ( so surprised how older I look
) but hey it is not about me, it is about an amazing mold material that many do not know how to use it. So hopefully this will help others
https://www.youtube.com/watch?v=le96sNV_b0Y&t=28s
https://www.youtube.com/watch?v=le96sNV_b0Y&t=28s
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: MM6
Enjoyed the video, can't wait for part 2.
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: MM6
Hi dear Brad, hope you are well. A while ago some artists were asking about how to work with Mold Mix 6 so I did this video and Zircar has 4 PDF's also to help others to be able to work with this casting material that has been part of my life for 30 years and I have loved working with it and hope others will now see how great it is.
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact: