Post by Jan de Jong »

Hello ! Is there in one of the books of Lundstrom a DIY for Universal Mould Release ? If yes....in which book ? Thank you for your help ! Jan de Jong (Holland)
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Books Lundstrom

Post by Kevin Midgley »

not that I know of.
It was originally a fusing ranch product.
If you can find it, buy it.
I suspect that the coat, but I have zero idea if my suspicion is correct and nor have I ever done any testing to see, is that it would be alumina hydrate.
A lot of fancy priced materials used for glass are commonly found cheaper at pottery supply places.
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Books Lundstrom

Post by Jan de Jong »

@ Kevin Midgley: Thank you for your information!
Difficult to find, so I try it now with this solution I ever read somewhere: Handsoap with water on the glazed ceramic.
Let dry and then the seperator. Jan
Jan de Jong
Posts: 114
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Books Lundstrom

Post by Jan de Jong »

For your information: no problems with the above mentioned procedure!! Everything Okay. Jan de Jong
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Books Lundstrom

Post by Kevin Midgley »

Brilliant idea. Not that I ever use commercially available objects for molds as I make all my own.
Of course there is one issue with using glazed ceramic plates for molds is that unless you are willing to drill air escape holes in them, you may have bubbles forming.
Vonon
Posts: 195
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Books Lundstrom

Post by Vonon »

I recall that the Universal Mold Release involved mixing something with common house paint. It could be coated directly over bowls, etc. that were already glazed such as plated or bowls you may already have. Don't remember what the "something" was.
Vonon
Vonon
Posts: 195
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Books Lundstrom

Post by Vonon »

I found Lundstrom's mold release at Fusion Headquarters.
https://www.fusionheadquarters.com/Univ ... molcoa.htm