Hi, gang.
I’m a new poster here, but have been lurking for years and deeply appreciate all of the wisdom posted here.
I think I have a bad relay in my kiln, but wanted to check with the experts to make sure I didn’t overlook any other potential problems.
I have a Paragon Janus 1613, which is a hybrid glass/ceramic top loader with elements in the walls and lid. In the most recent firing (in glass mode), I got a slow heating alarm, and noticed that the top element was not heating. After the kiln had cooled, I unplugged it and did a continuity test on the element that hadn’t heated. It tested out fine. Then I swapped the relay leads between the element that didn’t heat and another element that did heat properly. Now the top element heated normally, but the other one didn’t.
The kiln is three years old and has been used for maybe 150-200 firings, almost all of them glass firings.
The relay in question doesn’t show any visible damage.
Questions:
-Is there anything else I should try before I replace the relay? They’re pretty inexpensive, so I am inclined to go ahead and do it.
-The relay in question is a TE T92P7D22-12. Is there a better choice? I’m not going to build a controller box separate from the kiln, so I can’t use a part that’s highly heat-sensitive.
-Will it significantly help the relays last longer if I leave a fan pointing at the control box whenever the kiln is firing?
Thanks,
Mike
I think I have a bad relay. Am I doing this right?
Moderator: Tony Smith
-
michaelmace
- Posts: 3
- Joined: Sun Aug 16, 2020 9:16 pm
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: I think I have a bad relay. Am I doing this right?
Nothing will generally prevent a mechanical relay from eventually failing.
Firing at high temperatures with long holds where the relay clicks on and off more than once a minute WILL generally shorten a relay's life.
They will always fail in direct relationship with the importance of the glass in the kiln.
Firing at high temperatures with long holds where the relay clicks on and off more than once a minute WILL generally shorten a relay's life.
They will always fail in direct relationship with the importance of the glass in the kiln.
Re: I think I have a bad relay. Am I doing this right?
I would first call Paragon and ask them the question since they know the kiln the best.
There is more to life than increasing its speed.-Mahatma Gandhi
-
michaelmace
- Posts: 3
- Joined: Sun Aug 16, 2020 9:16 pm
Re: I think I have a bad relay. Am I doing this right?
Thank you both!