bubbles

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

bubbles

Post by Michael Stevens »

The glass that I purchase has a lot of micro bubbles and often folds, when I make beads I really don't want bubbles, but Even with a 20 minute bubble squeeze still has bubbles.

ify beads 12mm to 18mm size, have bubbles will a fire polish/ or fuse again and add a longer bubble squeeze of maybe 60. minutes will that remove pre existing bubbles
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: bubbles

Post by jim simmons »

I am sorry to inform you that if these are "micro"bubbles, then you are stuck with them unless you can figure
out a way to remelt the glass and hold for a long time.
The other Jim
Lynn Perry
Posts: 129
Joined: Sun Jun 08, 2003 5:27 pm
Location: East Tennessee

Re: bubbles

Post by Lynn Perry »

Bullseye considers the micro bubbles a "feature" of the handmade glass aspect. I think they also consider the "runs" on the top surface the same, but those certainly cause me a lot of problems when trying to match the gradient in dichroic glass.
Lynn Perry
Post Reply