I found this question here from long ago, but there was no response.
Boron Nitride spray is used as seperator on RVS.
But there is also POWDER. Had anyone try this ??  Jan
			
			
									
						
										
						Boron Nitride POWDER
Moderator: Tony Smith
- 
				Jan de Jong
 - Posts: 114
 - Joined: Sun Mar 09, 2003 3:31 pm
 - Location: The Netherlands
 
- 
				jim simmons
 - Posts: 478
 - Joined: Sun Mar 09, 2003 10:37 pm
 - Location: Hillsboro Oregon
 - Contact:
 
Re: Boron Nitride POWDER
Mix the powder with water to a cream consistency and paint it on like you would kiln wash.
I have used it on SS and clay fired stuff with good results.
The other Jim
			
			
									
						
										
						I have used it on SS and clay fired stuff with good results.
The other Jim
- 
				Jan de Jong
 - Posts: 114
 - Joined: Sun Mar 09, 2003 3:31 pm
 - Location: The Netherlands
 
Re: Boron Nitride POWDER
@ Jim Simmons: Thank you for your reply !!  Do you heat the SS  ( and Clay fired) ??  Jan
			
			
									
						
										
						- 
				jim simmons
 - Posts: 478
 - Joined: Sun Mar 09, 2003 10:37 pm
 - Location: Hillsboro Oregon
 - Contact:
 
Re: Boron Nitride POWDER
nope. treat it just like it is a product called  "ZYP".
paint it on, let it dry for about 30 min. and you are good to go.
The Other Jim
			
			
									
						
										
						paint it on, let it dry for about 30 min. and you are good to go.
The Other Jim
- 
				Jan de Jong
 - Posts: 114
 - Joined: Sun Mar 09, 2003 3:31 pm
 - Location: The Netherlands
 
Re: Boron Nitride POWDER
@ Jim:  Thank you  ! I PM you for another question.  Jan