Hello,  not knowing about this notation of COE. I think it is COE 96 ....am I right ?
COE (9,60 +- 0,15) x 10  -6         Sorry, don 't know how to make this signs in the right way.  Jan
			
			
									
						
										
						Reading COE
Moderator: Tony Smith
- 
				Lynn Perry
 - Posts: 129
 - Joined: Sun Jun 08, 2003 5:27 pm
 - Location: East Tennessee
 
Re: Reading COE
Hi Jan.  When I read your question, I thought this should be easy to find with Google.  It was not, because the actual measurement has been lost to the reduced reporting of 90, 96, 82. etc.  I finally found the answer in an earlier post on the board:
http://warmglass.com/phpBB3/viewtopic.php?t=41565
Look at the very bottom of the thread. So, 9.6x10-6 is the same as 96x10-5 and 96 COE, I think.....
			
			
									
						
							http://warmglass.com/phpBB3/viewtopic.php?t=41565
Look at the very bottom of the thread. So, 9.6x10-6 is the same as 96x10-5 and 96 COE, I think.....
Lynn Perry
			
						- 
				Jan de Jong
 - Posts: 114
 - Joined: Sun Mar 09, 2003 3:31 pm
 - Location: The Netherlands
 
Re: Reading COE
@ Lynn Perry: Thank you  !   Jan